Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing Home Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing Departments Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing Bulletin Board Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing About Us Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing Help Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing

 

     
   
Surface Turbulence

Velocities higher than 0.5 m/s into the mould cavity will cause the melt to jet into the mould, creating oxide and bubble damage in the casting. Properties, leak tightness, and corrosion resistance will all be randomly degraded in proportion to any excess velocity.

Read more about the relationship of melt speed, turbulence, and casting quality in part two of "Ten Rules for Good Castings"

"Ten Rules for Good Castings" ©2001 John Campbell. All rights reserved.
   
   
 
 