Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing Home Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing Departments Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing Bulletin Board Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing About Us Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing Help Casting Trade, casting processes, investment casting, sand casting, die casting, tooling, mold, mould, foundry, pattern, finishing

 

     
   
Core Blow

The outgassing of cores can lead to huge defects, filling whole areas of the tops of castings. However, even a small blow from a core can leave a bubble trail that can create a leak defect.

Read more about the impact of core blows on castings in part five of "Ten Rules for Good Castings".

"Ten Rules for Good Castings" ©2001 John Campbell. All rights reserved.
   
   
 
 


Copyrights 2000 - 2007 (c) CastingTrade.com Inc.